DC01 Plate Cold Rolled Steel Sheet

It is a non-alloy cold-rolled steel with very low carbon content. It is often used in the automotive industry and for making electronic components. The low carbon content of this steel makes it very easy to work with. It can be welded, brazed and soldered without any issues.

Giơi thiệu sản phẩm

Giơi thiệu sản phẩm

 

DC01 Plate:

DC01 represents the basic grade of the DC steel family and is also known under the former designations St12 or FeP01. This grade can be used for simple forming operations such as bending, coining, beading and drawing.

 

DC01 steel (1.0330 material) is a European standard cold-rolled quality low-carbon steel flat product for cold forming. In BS and DIN EN 10130 standard, it contains 5 other steel grades: DC03 (1.0347), DC04 (1.0338), DC05 (1.0312), DC06 ( 1.0873) and DC07 (1.0898), the surface quality is divided into 2 types: DC01-A and DC01-B. In addition, this steel is also used under electrogalvanizing conditions. The designation of the steel is DC01+ZE (or 1.0330+ZE), and the standard is EN 10152.

 

T/T, L/C, Paypal, Western Union. and Generally it is 30% prepayment, 70% balance see B/L copy, or 100% LC at sight.
0.2mm-300mm or as customer requirement
500mm-3000mm or customize
1000mm-12000mm or as buyer needs
Thickness: +/-0.02mm, Width:+/-2mm
One-stop service
20000ton/month
508mm or 610mm

 

DC01 is a cold-rolled steel plate, which is defined in the Chinese standard GBT 5213-2008 cold-rolled low-carbon steel plate and steel strip. DC01 corresponds to Q195L and No. 10 steel or No. 8 steel.

 

Chemical composition of DC01 steel plate:

 

1. Carbon C: Less than or equal to 0.12

2. Manganese Mn: Less than or equal to 0.60

3. Sulfur S: allowable residual content Less than or equal to 0.045

4. Phosphorus P: allowable residual content Less than or equal to 0.045

5. Alt (Al total): allowable residual content Greater than or equal to 0.020

 

DC01 cold plate European standard brand corresponding to EPSA standard B53 3106 Corresponding China substitute material WIF DC01 bare board WISCO Baosteel DC5D+Z galvanized Dalian TAG DX5D+Z

 